+ PU Casting Elastomer Prepolymer
+ Casting PU
+ PU Casting Prepolymer
+ Castable PU
+ PU (Polyurethane) prepolymer for casting polyurethane elastomer parts
+ Cast Polyurethane Resin
+ Castable Polyurethane
+ PU prepolymer for casting
+ PU elastomer Prepolymer
+ Casting PU Resin
+ Casting PU Prepolymer
+ Casting PU Elastomer
Application | |||
---|---|---|---|
Bushes, Castor Wheels, Couplings, Conveyor Rollers, Cutting Boards, Fork-lift Tyres, Gears, Grading Screens, Pneumatic and Oil Seals, Scrapers, Skate Wheels, Wire Guides. |
Introduction | |||
---|---|---|---|
"PU Casting Elastomer" hot cast urethane can be cured by reacting with a polyamine or a polyol hardener. The molding process is composed of pre-heating, degassing, mixing with a hardener, pouring into the mold, curing, demolding and post curing. |
PPG + MDI hot cast urethane | ||||
---|---|---|---|---|
CPU-MG-1070 | CPU-MG-1080 | CPU-MG-1090 | CPU-MG-1095 | |
Hardness (Shore A) | 70 ± 3 | 80 ± 2 | 90 ± 2 | 95 ± 2 |
NCO Content (%) | 5.8 ± 0.2 | 6.5 ± 0.2 | 8.9 ± 0.2 | 9.2 ± 0.2 |
Viscosity, Poise (100℃) | - | - | - | - |
1.4 Butane Diol (pph) | 5.80 | 6.61 | 9.16 | 9.41 |
Working Temperature (Prepolymer) (℃) | 80 | 80 | 80 | 80 |
Pot-Life (Min) | 5 | 4.5 | 4 | 3-5 |
Tensile Strength (psi) | 2100-2600 | 2200-2900 | 3200-3800 | 4800-6000 |
Elongation (%) | 600-700 | 500-650 | 450-600 | 400-520 |
Tear Strength (pli) | 250-300 | 300-355 | 410-470 | 305-350 |
Notice: These values are based on the test of our present laboratory test specimens. |